Nickel 200/201
C-276
Alloy 400
Alloy 600
Alloy 601
Alloy 625
Alloy 800H/800HT
Alloy 825
Nickel 200/201

Nickel 200

  • UNS N02200
  • WERKSTOFF 2.4066 / 2.4060

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureNickel 200
Tensile Strengthksi65
0.2% Yield Strengthksi30
Elongation%45
HardnessHV110

Composition

ElementNickel 200
NiNickel99.00% min
FeIron0.40% max
MnManganese0.35% max
SiSilicon0.35% max
CuCopper0.25% max
CCarbon0.15% max
SSulfer0.01% max

Nickel 201

  • UNS N02201
  • WERKSTOFF 2.4066 / 2.4060

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureNickel 201
Tensile Strengthksi60
0.2% Yield Strengthksi35
Elongation%50
HardnessHV10

Composition

Element Nickel 201
NiNickel99.00% min
FeIron0.40% max
MnManganese0.35% max
SiSilicon0.35% max
CuCopper0.25% max
CCarbon0.02% max
SSulfer0.01% max
C-276

C-276

  • UNS N10276
  • WERKSTOFF 2.4819

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureC-276
Tensile Strengthksi110
0.2% Yield Strengthksi50
Elongation%60
HardnessHV180

Composition

ElementC-276
NiNickelBalance
MoMolybdenum15.00% - 17.00%
CrChromium14.50% - 16.50%
FeIron4.00% - 7.00%
WTungsten3.00% - 4.00%
CoCobalt2.50% max
MnManganese1.00% max
VVanadium0.35% max
SiSilicon0.08% max
PPhosphorus0.04% max
SSulfer0.03% max
CCarbon0.01% max
Alloy 400

Alloy 400

  • UNS N04400
  • WERKSTOFF 2.4360 / 2.4361

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureAlloy 400
Tensile Strengthksi80
0.2% Yield Strengthksi40
Elongation%45
HardnessHV140

Composition

Element Alloy 400
NiNickel63.00% min
CuCopper28%-34% max
FeIron2.50% max
MnManganese2.00% max
SiSilicon0.50% max
CCarbon0.30% max
SSulfer0.02% max
Alloy 600

Alloy 600

  • UNS N06600
  • WERKSTOFF 2.4816

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureAlloy 600
Tensile Strengthksi100
0.2% Yield Strengthksi40
Elongation%40
HardnessHV170

Composition

Element Alloy 600
NiNickel72.00% min
CrChromium14.00%-17.00% max
FeIron6.00%-10.00% max
MnManganese1.00% max
SiSilicon0.50% max
CuCopper0.50% max
CCarbon0.15% max
SSulfer0.01% max
Alloy 601

Alloy 601

  • UNS N06601
  • WERKSTOFF 2.4851

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureAlloy 601
Tensile Strengthksi95
0.2% Yield Strengthksi40
Elongation%50
HardnessHV145

Composition

Element Alloy 601
NiNickel58.00% -63.00%
CrChromium21.00%-25.00%
FeIronBalance
AlAluminum1.00% -1.70%
MnManganese1.00% max
CuCopper1.00% max
SiSilicon0.50% max
CCarbon0.10% max
SSulfer0.01% max
Alloy 625

Alloy 625

  • UNS N06625
  • WERKSTOFF 2.4856

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureAlloy 625
Tensile Strengthksi125
0.2% Yield Strengthksi70
Elongation%50
HardnessHV200

Composition

Elements Alloy 625
NiNickel58.00% min
CrChromium20.00% - 23.00%
MoMolybdenum8.00% - 10.00%
FeIron5.00% max
Nb + TaNiobium + Tantalum3.15% - 4.15%
CoCobalt1.00% max
MnManganese0.50% max
SiSilicon0.50% max
AlAluminum0.40% max
TiTitanium0.40% max
CCarbon0.10% max
SSulfer0.01% max
PPhosphorus0.01% max
Alloy 800H/800HT

Alloy 800H

  • UNS N08810
  • WERKSTOFF 1.4958

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureAlloy 800H
Tensile Strengthksi80
0.2% Yield Strengthksi35
Elongation%45
HardnessHV145

Composition

Element Alloy 800H
FeIron39.50% min
NiNickel30.00% - 35.00%
CrChromium19.00% - 23.00%
MnManganese1.50% max
SiSilicon1.00% max
CuCopper0.75% max
Al + TiAluminum + Titanium0.30% - 1.20%
TiTitanium0.15% - 0.60%
AlAluminum0.15% - 0.60%
CCarbon0.05% - 0.10%
SSulfer0.01% max

Alloy 800HT

  • UNS N08811
  • WERKSTOFF 1.4876 / 1.4959

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureAlloy 800HT
Tensile Strengthksi80
0.2% Yield Strengthksi35
Elongation%45
HardnessHV145

Composition

Element Alloy 800HT
FeIron39.50% min
NiNickel30.00% - 35.00%
CrChromium19.00% - 23.00%
MnManganese1.50% max
SiSilicon1.00% max
Al + TiAluminum + Titanium0.85% - 1.20%
CuCopper0.75% max
CCarbon0.06% - 0.10%
TiTitanium0.25% - 0.60%
AlAluminum0.25% - 0.60%
SSulfer0.01% max
Alloy 825

Alloy 825

  • UNS N08825
  • WERKSTOFF 2.4858

*Nominal Room Temperature Mechanical Properties. Typical Data. Not suitable for design or specifications.

Key Properties* (in annealed condition)

PropertiesUnit of MeasureAlloy 825
Tensile Strengthksi95
0.2% Yield Strengthksi45
Elongation%45
HardnessHV155

Composition

Element Alloy 825
NiNickel38.00% - 46.00%
FeIron22.00% min
CrChromium19.50% - 23.50%
MoMolybdenum2.50% - 3.50%
CuCopper1.50% - 3.00%
MnManganese1.00% max
TiTitanium0.60% - 1.20%
SiSilicon0.50% max
AlAluminum0.20% max
CCarbon0.05% max
SSulfer0.03% max